Keltan® has the broadest portfolio of premium EP(D)M grades in the world. The versatility of Keltan® elastomer, high product quality, high supply reliability and high service level enables high performance for our customers, their products and industrial solutions.

Keltan® 0500R Downsheared
Property Nominal Value Test Method Condition Temperature
Melt Flow Index 190 °C 11 g/10mi ASTM D 1238
Molecular Weight Distribution Narrow Internal Method
Ethylene Content 49 wt % ASTM D 3900
Keltan® 2450 Low Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 28 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 48 wt % ASTM D 3900
ENB Content 4,1 wt % ASTM D 6047
Keltan® 2650 Low Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 25 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 53 wt % ASTM D 3900
ENB Content 6,0 wt % ASTM D 6047
Keltan® 2650C Low Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 25 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 46 wt % ASTM D 3900
ENB Content 6,0 wt % ASTM D 6047
Keltan® 2750 Low Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 28 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 48 wt % ASTM D 3900
ENB Content 7,8 wt % ASTM D 6047
Keltan® 4450 Medium Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 46 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution Narrow Internal Method
Ethylene Content 52 wt % ASTM D 3900
ENB Content 4,3 wt % ASTM D 6047
Keltan® 4450S Medium Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 42 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 52 wt % ASTM D 3900
ENB Content 4,3 wt % ASTM D 6047
Keltan® 4460D Medium Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 46 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution Broad Internal Method
Ethylene Content 58 wt % ASTM D 3900
DCPD Content 4,5 wt % ASTM D 6047

 Hydrogenated Nitrile Butadiene Rubber

Successful in many key industries. Excellent properties e.g. for engine components. Reliable resistance to aggressive fluids, oil and grease – able to function up to 165°C.

Therban® 3446 Partially Saturated (suitable for peroxide and sulfur crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 61 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34,0 wt % ISO 24698-1
Residual Double Bonds 3,95 % IR Spectroscopy
Therban® AT LT 2004 VP Low Mooney – Advanced Technology Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 39 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 21,0 wt % ISO 24698-1
Residual Double Bonds 0,9 % Internal Method

Nitrile Butadiene Rubber

ARLANXEO NBR clearly sets itself apart from other synthetic rubbers not only with regard to its oil resistance but also regarding its other strong properties. In addition to the key properties of our trademark products Perbunan® and Krynac®, processability is a further extremely important...

Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 115 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 38,0 wt % ISO 24698