Find Products

19 results

Regular & halogenated butyl rubber

The X_Butyl® product family contains a broad range of regular butyl rubber products and halogenated butyl rubber products.

Bromobutyl Rubber
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 39 MU ISO 289 / ASTM D 1646 ML (1+8) 125 °C
Bromine Content 1,80 wt % Internal Method
Antioxidant non-staining ≥ 0,03 wt % (*)
Ash Content ≤ 0,7 wt % ISO 247 / ASTM D 5667
Volatile Content ≤ 0,7 wt % ISO 248 / ASTM D 5668
Bromobutyl Rubber
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 32 MU ISO 289 / ASTM D 1646 ML (1+8) 125 °C
Bromine Content 1,80 wt % Internal Method
Antioxidant non-staining > 0,03 wt % Internal Method
Bromobutyl Rubber
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 46 MU ISO 289 / ASTM D 1646 ML (1+8) 125 °C
Bromine Content 1,80 wt % Internal Method
Antioxidant non-staining > 0,03 wt % Internal Method
Ash Content ≤ 0,7 wt % ISO 247 / ASTM D 5667
Volatile Content ≤ 0,7 wt % ISO 248 / ASTM D 5668
Chlorobutyl Rubber
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 38 MU ISO 289 / ASTM D 1646 ML (1+8) 125 °C
Chlorine Content 1,25 wt % Internal Method
Antioxidant non-staining ≥ 0,03 wt % (*)
Ash Content ≤ 0,5 wt % ISO 247 / ASTM D 5667
Volatile Content ≤ 0,5 wt % ISO 248 / ASTM D 5668

Butadiene Rubber

The BR polymer family contains polybutadiene rubbers which are divided into different categories according to their polymerization process and application field.

Neodymium BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 63 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Neodymium BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 44 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Cobalt BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 53 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Cobalt BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 40 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Cobalt BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 43 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Neodymium BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 44 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Easy Processing Nd-BR (Buna Nd)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 63 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Easy Processing Nd-BR (Buna Nd)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 44 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %

Emulsion Styrene Butadiene Rubber

The Buna® SE product group comprises the general purpose emulsion styrene-butadiene rubbers (E-SBR) which is one of the most important types of synthetic rubber. Emulsion Styrene Butadiene Rubber is the most widely used rubber in the world, representing about 40% of the synthetic rubber market,...

Oil-free E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 52 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775
Oil-free E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 53 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775
Oil-free E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 49 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775

Ethylene Propylene Diene Rubber

Keltan® has the broadest portfolio of premium EP(D)M grades in the world. The versatility of Keltan® elastomer, high product quality, high supply reliability and high service level enables high performance for our customers, their products and industrial solutions.

Low Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 33 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution Narrow Internal Method
Ethylene Content 55 wt % ASTM D 3900
ENB Content 2,3 wt % ASTM D 6047
Medium Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 46 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution Broad Internal Method
Ethylene Content 58 wt % ASTM D 3900
DCPD Content 4,5 wt % ASTM D 6047
Low Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 36 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 68 wt % ASTM D 3900
ENB Content 4,6 wt % ASTM D 6047

Ethylene Vinyl Acetate Rubber

Durability energized by Levapren® rubber from ARLANXEO. The cost-effective EVM-specialty fordemanding applications as for moving sidewalks and floorings.

General Purpose Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 27 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Vinyl Acetate Content 70 wt % Internal Method LP 015