Emulsion Styrene Butadiene Rubber

The Buna® SE product group comprises the general purpose emulsion styrene-butadiene rubbers (E-SBR) which is one of the most important types of synthetic rubber. Emulsion Styrene Butadiene Rubber is the most widely used rubber in the world, representing about 40% of the synthetic rubber market,...

Oil-free E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 52 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775
Oil-free E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 49 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775

Ethylene Vinyl Acetate Rubber

Durability energized by Levapren® rubber from ARLANXEO. The cost-effective EVM-specialty fordemanding applications as for moving sidewalks and floorings.

General Purpose Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 27 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Vinyl Acetate Content 50 wt % Internal Method LP 015
General Purpose Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 27 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Vinyl Acetate Content 60 wt % Internal Method LP 015
General Purpose Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 27 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Vinyl Acetate Content 70 wt % Internal Method LP 015
General Purpose Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 38 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Vinyl Acetate Content 90 wt % Internal Method LP 015

 Hydrogenated Nitrile Butadiene Rubber

Successful in many key industries. Excellent properties e.g. for engine components. Reliable resistance to aggressive fluids, oil and grease – able to function up to 165°C.

Partially Saturated (suitable for peroxide and sulfur crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 61 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34,0 wt % ISO 24698-1
Residual Double Bonds 3,95 % IR Spectroscopy
Fully Saturated (suitable for peroxide crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 70 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34,0 wt % ISO 24698-1
Residual Double Bonds 0,9 % IR Spectroscopy

Functionalized & Standard S-SBR and Block Co-Polymers

The Buna® S-SBR product family contains a wide range of solution styrene butadiene rubber products which are defined into Buna FX, Buna VSL, Buna SL and Buna BL.

Diblock Copolymers (Buna BL)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 45 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 48,0 wt % ASTM D 5775
Block Styrene Content 30,0 wt % ASTM D 3314
Diblock Copolymers (Buna BL)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 50 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 48,5 wt % ASTM D 5775
Block Styrene Content 34,5 wt % ASTM D 3314
Standard S-SBR (Buna SL)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 45 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Styrene Content 25 wt % ASTM D 5775