Butadiene Rubber

The BR polymer family contains polybutadiene rubbers which are divided into different categories according to their polymerization process and application field.

Easy Processing Nd-BR (Buna Nd)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 44 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %

Emulsion Styrene Butadiene Rubber

The Buna® SE product group comprises the general purpose emulsion styrene-butadiene rubbers (E-SBR) which is one of the most important types of synthetic rubber. Emulsion Styrene Butadiene Rubber is the most widely used rubber in the world, representing about 40% of the synthetic rubber market,...

Oil-free E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 52 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775
Oil-free E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 53 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775
Oil-free E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 49 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775

Ethylene Propylene Diene Rubber

Keltan® has the broadest portfolio of premium EP(D)M grades in the world. The versatility of Keltan® elastomer, high product quality, high supply reliability and high service level enables high performance for our customers, their products and industrial solutions.

Low Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 54 MU ISO 289 / ASTM D 1646 ML (1+8) 100 °C
Molecular Weight Distribution Medium Internal Method
Ethylene Content 56 wt % ASTM D 3900
ENB Content 11,0 wt % ASTM D 6047
Low Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 25 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution Very broad Internal Method
Ethylene Content 60 wt % ASTM D 3900
ENB Content 6,3 wt % ASTM D 6047
Medium Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 48 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution Broad Internal Method
Ethylene Content 56 wt % ASTM D 3900
ENB Content 4,1 wt % ASTM D 6047
Oil Content 50 PHR ISO 1407
Medium Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 55 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 70 wt % ASTM D 3900
ENB Content 4,6 wt % ASTM D 6047
High Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 63 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 64 wt % ASTM D 3900
ENB Content 4,8 wt % ASTM D 6047
High Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 70 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution Narrow Internal Method
Ethylene Content 67 wt % ASTM D 3900
ENB Content 4,7 wt % ASTM D 6047
Very high Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 66 MU ISO 289 / ASTM D 1646 ML (1+8) 150 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 56 wt % ASTM D 3900
ENB Content 6,5 wt % ASTM D 6047
High Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 80 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 55 wt % ASTM D 3900
ENB Content 5,5 wt % ASTM D 6047
High Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 80 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 66 wt % ASTM D 3900
ENB Content 5,0 wt % ASTM D 6047
High Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 80 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 48 wt % ASTM D 3900
ENB Content 5,5 wt % ASTM D 6047