Butadiene Rubber

The BR polymer family contains polybutadiene rubbers which are divided into different categories according to their polymerization process and application field.

Cobalt BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 53 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Cobalt BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 40 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Neodymium BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 63 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Neodymium BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 37 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Oil Content 27,3 wt % ISO 1407
Cis 1,4 Content > 96 %
Cobalt BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 43 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Easy Processing Nd-BR (Buna Nd)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 63 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Neodymium BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 44 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Easy Processing Nd-BR (Buna Nd)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 44 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Neodymium BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 37 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Oil Content 27,3 wt % ISO 1407
Cis 1,4 Content > 96 %
Neodymium BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 44 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %

Emulsion Styrene Butadiene Rubber

The Buna® SE product group comprises the general purpose emulsion styrene-butadiene rubbers (E-SBR) which is one of the most important types of synthetic rubber. Emulsion Styrene Butadiene Rubber is the most widely used rubber in the world, representing about 40% of the synthetic rubber market,...

Oil-extended E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 53 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 40,0 wt % ASTM D 5775
Oil Content 27,2 wt % ASTM D 5774
Oil-free E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 52 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775
Oil-free E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 53 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775
Oil-extended E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 50 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775
Oil Content 27,2 wt % ASTM D 5774
Oil-free E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 49 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775
Oil-extended E-SBR
Oil-extended E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 49 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775
Oil Content 27,2 wt % ASTM D 5774
Oil-extended E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 51 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 23,5 wt % ASTM D 5775
Oil Content 27,2 wt % ASTM D 5774
Oil-extended E-SBR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 55 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Bound Styrene 40,0 wt % ASTM D 5775
Oil Content 27,2 wt % ASTM D 5774

Functionalized & Standard S-SBR and Block Co-Polymers

The Buna® S-SBR product family contains a wide range of solution styrene butadiene rubber products which are defined into Buna FX, Buna VSL, Buna SL and Buna BL.

Functionalized S-SBR (Buna FX)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 63 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Styrene Content 34 wt % Internal Method
Oil Content 75 PHR 27,3 wt % Internal Method
Vinyl Content 32 wt % Internal Method
Standard S-SBR (Buna SL)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 45 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Styrene Content 18 wt % ASTM D 5775
Oil Content 27,3 wt % ASTM D 5774
Standard S-SBR (Buna VSL)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 80 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Styrene Content 38 wt % Internal Method
Oil Content 27,3 wt % Internal Method
Vinyl Content 24 wt % Internal Method
Standard S-SBR (Buna VSL)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 66 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Styrene Content 38 wt % Internal Method
Oil Content 27,3 wt % Internal Method
Vinyl Content 30 wt % Internal Method
Standard S-SBR (Buna VSL)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 50 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Styrene Content 38 wt % Internal Method
Oil Content 27,3 wt % Internal Method
Vinyl Content 25 wt % Internal Method
Standard S-SBR (Buna VSL)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 50 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Styrene Content 26 wt % Internal Method
Oil Content 27,3 wt % Internal Method
Vinyl Content 44,5 wt % Internal Method
Standard S-SBR (Buna VSL)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 62 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Styrene Content 26 wt % Internal Method
Oil Content 27,3 wt % Internal Method
Vinyl Content 44,5 wt % Internal Method
Functionalized S-SBR (Buna FX)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 65 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Styrene Content 34 wt % Internal Method
Oil Content 27,3 wt % Internal Method
Vinyl Content 32 wt % Internal Method
Standard S-SBR (Buna SL)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 75 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Styrene Content 18 wt % Internal Method
Oil Content 13 wt % ASTM D 5774
Standard S-SBR (Buna SL)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 45 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Styrene Content 25 wt % ASTM D 5775