Find Products

42 results

Butadiene Rubber

The BR polymer family contains polybutadiene rubbers which are divided into different categories according to their polymerization process and application field.

Buna® CB 1203 Cobalt BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 43 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Buna® CB 1220 AO Cobalt BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 40 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Buna® CB 1221 Cobalt BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 53 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %

Ethylene Propylene Diene Rubber

Keltan® has the broadest portfolio of premium EP(D)M grades in the world. The versatility of Keltan® elastomer, high product quality, high supply reliability and high service level enables high performance for our customers, their products and industrial solutions.

Keltan 8850C High Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 80 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 48 wt % ASTM D 3900
ENB Content 5,5 wt % ASTM D 6047
Keltan® 13561C Very high Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 92 MU ISO 289 / ASTM D 1646 ML (1+8) 150 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 56 wt % ASTM D 3900
ENB Content 5,5 wt % ASTM D 6047
Oil Content 15 PHR ISO 1407
Keltan® 2450 Low Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 28 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 48 wt % ASTM D 3900
ENB Content 4,1 wt % ASTM D 6047

Ethylene Vinyl Acetate Rubber

Durability energized by Levapren® rubber from ARLANXEO. The cost-effective EVM-specialty fordemanding applications as for moving sidewalks and floorings.

Levapren 600 XL VP Special Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 55 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Vinyl Acetate Content 60 wt % Internal Method LP 015
Levapren 700 XL VP Special Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 60 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Vinyl Acetate Content 70 wt % Internal Method LP 015
Levapren® 600 General Purpose Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 27 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Vinyl Acetate Content 60 wt % Internal Method LP 015
Levapren® 700 General Purpose Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 27 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Vinyl Acetate Content 70 wt % Internal Method LP 015
Levapren® 700 PXL VP Special Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 60 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Vinyl Acetate Content 70 wt % Internal Method LP 015

 Hydrogenated Nitrile Butadiene Rubber

Successful in many key industries. Excellent properties e.g. for engine components. Reliable resistance to aggressive fluids, oil and grease – able to function up to 165°C.

Therban® 3406 Fully Saturated (suitable for peroxide crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 63 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34 wt % ISO 24698-1
Residual Double Bonds 0,9 % IR Spectroscopy
Therban® 3407 Fully Saturated (suitable for peroxide crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 70 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34,0 wt % ISO 24698-1
Residual Double Bonds 0,9 % IR Spectroscopy
Therban® 3446 Partially Saturated (suitable for peroxide and sulfur crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 61 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34,0 wt % ISO 24698-1
Residual Double Bonds 3,95 % IR Spectroscopy
Therban® 3467 Partially Saturated (suitable for peroxide and sulfur crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 68 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34,0 wt % ISO 24698-1
Residual Double Bonds 5,5 % IR Spectroscopy
Therban® 3607 Fully Saturated (suitable for peroxide crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 66 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 36,0 wt % ISO 24698-1
Residual Double Bonds 0,9 % IR Spectroscopy
Therban® 3627 Partially Saturated (suitable for peroxide and sulfur crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 66 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 36,0 wt % ISO 24698-1
Residual Double Bonds 2,0 % IR Spectroscopy
Therban® 3629 Partially Saturated (suitable for peroxide and sulfur crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 87 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 36,0 wt % ISO 24698-1
Residual Double Bonds 2,0 % IR Spectroscopy
Therban® 3668 VP Partially Saturated (suitable for peroxide and sulfur crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 80 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 36,0 wt % ISO 24698-1
Residual Double Bonds 6,0 % IR Spectroscopy
Therban® 3907 Fully Saturated (suitable for peroxide crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 70 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 39,0 wt % ISO 24698-1
Residual Double Bonds 0,9 % IR Spectroscopy
Therban® 4307 Fully Saturated (suitable for peroxide crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 63 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 42,5 wt % ISO 24698-1
Residual Double Bonds 0,9 % IR Spectroscopy

Nitrile Butadiene Rubber

ARLANXEO NBR clearly sets itself apart from other synthetic rubbers not only with regard to its oil resistance but also regarding its other strong properties. In addition to the key properties of our trademark products Perbunan® and Krynac®, processability is a further extremely important...

Krynac® 2645 F Medium Cure
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 45 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 26,0 wt % ISO 24698
Krynac® XL 3355 Pre-Crosslinked
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 55 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 33,0 wt % ISO 24698
Perbunan® 2845 F Fast Cure
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 45 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 28,0 wt % ISO 24698
Perbunan® 2870 F Fast Cure
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 70 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 28,0 wt % ISO 24698