Butadiene Rubber

The BR polymer family contains polybutadiene rubbers which are divided into different categories according to their polymerization process and application field.

Neodymium BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 63 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Neodymium BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 44 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Cobalt BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 53 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Cobalt BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 40 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Cobalt BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 43 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Neodymium BR
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 44 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %
Easy Processing Nd-BR (Buna Nd)
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 63 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Cis 1,4 Content > 96 %

Ethylene Propylene Diene Rubber

Keltan® has the broadest portfolio of premium EP(D)M grades in the world. The versatility of Keltan® elastomer, high product quality, high supply reliability and high service level enables high performance for our customers, their products and industrial solutions.

High Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 65 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 44 wt % ASTM D 3900
ENB Content 9,0 wt % ASTM D 6047
High Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 61 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution Medium Internal Method
Ethylene Content 65,6 wt % ASTM D 3900
ENB Content 6,3 wt % ASTM D 6047
Oil Content 50 PHR ISO 1407

 Hydrogenated Nitrile Butadiene Rubber

Successful in many key industries. Excellent properties e.g. for engine components. Reliable resistance to aggressive fluids, oil and grease – able to function up to 165°C.

Partially Saturated (suitable for peroxide and sulfur crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 55 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34,0 wt % ISO 24698-1
Residual Double Bonds 18,0 % IR Spectroscopy
Partially Saturated (suitable for peroxide and sulfur crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 68 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34,0 wt % ISO 24698-1
Residual Double Bonds 5,5 % IR Spectroscopy
Fully Saturated (suitable for peroxide crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 63 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34 wt % ISO 24698-1
Residual Double Bonds 0,9 % IR Spectroscopy
Partially Saturated (suitable for peroxide and sulfur crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 61 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34,0 wt % ISO 24698-1
Residual Double Bonds 3,95 % IR Spectroscopy
Partially Saturated (suitable for peroxide and sulfur crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 80 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 36,0 wt % ISO 24698-1
Residual Double Bonds 6,0 % IR Spectroscopy
Fully Saturated (suitable for peroxide crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 70 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34,0 wt % ISO 24698-1
Residual Double Bonds 0,9 % IR Spectroscopy
Partially Saturated (suitable for peroxide and sulfur crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 97 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 43,0 wt % ISO 24698-1
Residual Double Bonds 5,5 % IR Spectroscopy
Fully Saturated (suitable for peroxide crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 70 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 39,0 wt % ISO 24698-1
Residual Double Bonds 0,9 % IR Spectroscopy
Special Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 22 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34,0 wt % ISO 24698-1
Residual Double Bonds 5,5 % IR Spectroscopy
Low Mooney – Advanced Technology Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 39 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 34,0 wt % ISO 24698-1
Residual Double Bonds 0,9 % IR Spectroscopy

Nitrile Butadiene Rubber

ARLANXEO NBR clearly sets itself apart from other synthetic rubbers not only with regard to its oil resistance but also regarding its other strong properties. In addition to the key properties of our trademark products Perbunan® and Krynac®, processability is a further extremely important...

High Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 95 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 28,0 wt % ISO 24698
High Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 110 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 33,0 wt % ISO 24698
Plasticizer Extended
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 33 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 22,0 wt % ISO 24698
High Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 120 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 28,0 wt % ISO 24698