Ethylene Propylene Diene Rubber

Keltan® has the broadest portfolio of premium EP(D)M grades in the world. The versatility of Keltan® elastomer, high product quality, high supply reliability and high service level enables high performance for our customers, their products and industrial solutions.

Medium Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 52 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 58 wt % ASTM D 3900
ENB Content 4,5 wt % ASTM D 6047
Oil Content 100 PHR ISO 1407
High Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 80 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 66 wt % ASTM D 3900
ENB Content 5,0 wt % ASTM D 6047
High Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 80 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 48 wt % ASTM D 3900
ENB Content 5,5 wt % ASTM D 6047
Medium Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 48 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution Broad Internal Method
Ethylene Content 56 wt % ASTM D 3900
ENB Content 4,1 wt % ASTM D 6047
Oil Content 50 PHR ISO 1407
Medium Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 48 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 64 wt % ASTM D 3900
ENB Content 8,7 wt % ASTM D 6047
Oil Content 100 PHR ISO 1407
Medium Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 48 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 62 wt % ASTM D 3900
ENB Content 8,7 wt % ASTM D 6047
Oil Content 100 PHR ISO 1407
Medium Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 46 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution Narrow Internal Method
Ethylene Content 66 wt % ASTM D 3900
ENB Content 5,1 wt % ASTM D 6047
Oil Content 75 PHR ISO 1407
Medium Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 52 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution CLCB Internal Method
Ethylene Content 58 wt % ASTM D 3900
ENB Content 4,5 wt % ASTM D 6047
Oil Content 75 PHR ISO 1407
Medium Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 37 MU ISO 289 / ASTM D 1646 ML (1+8) 150 °C
Molecular Weight Distribution Narrow Internal Method
Ethylene Content 64 wt % ASTM D 3900
ENB Content 4,0 wt % ASTM D 6047
Oil Content 50 PHR ISO 1407
High Mooney
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 63 MU ISO 289 / ASTM D 1646 ML (1+4) 125 °C
Molecular Weight Distribution Medium Internal Method
Ethylene Content 64 wt % ASTM D 3900
DCPD Content 1,2 wt % ASTM D 6047

 Hydrogenated Nitrile Butadiene Rubber

Successful in many key industries. Excellent properties e.g. for engine components. Reliable resistance to aggressive fluids, oil and grease – able to function up to 165°C.

Partially Saturated (suitable for peroxide and sulfur crosslinking) Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 61 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 43,0 wt % ISO 24698-1
Residual Double Bonds 5,5 % IR Spectroscopy
Low Temperature Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 74 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Acrylonitrile Content 21,0 wt % ISO 24698-1
Residual Double Bonds 0,9 % IR Spectroscopy