Ethylene Vinyl Acetate Rubber

Durability energized by Levapren® rubber from ARLANXEO. The cost-effective EVM-specialty fordemanding applications as for moving sidewalks and floorings.

Thermoplast Modification Grades
Thermoplast Modification Grades
Property Nominal Value Test Method Condition Temperature
Melt Flow Index 190 °C 3 g/10mi ASTM D 1238
Vinyl Acetate Content 45 wt % Internal Method LP 015
Separating Agent ≤ 0.8 wt % 7 wt % ISO 247 / ASTM D 5667
General Purpose Grades
Property Nominal Value Test Method Condition Temperature
Melt Flow Index 190 °C 25 g/10mi ISO 1133
Vinyl Acetate Content 45 wt % Internal Method LP 015
General Purpose Grades
Property Nominal Value Test Method Condition Temperature
Melt Flow Index 190 °C 3 g/10mi ISO 1133
Vinyl Acetate Content 45 wt % Internal Method LP 015
General Purpose Grades
Property Nominal Value Test Method Condition Temperature
Melt Flow Index 190 °C 25 g/10mi ISO 1133
Vinyl Acetate Content 68 wt % Internal Method LP 015
General Purpose Grades
Property Nominal Value Test Method Condition Temperature
Melt Flow Index 190 °C 2,75 g/10mi ISO 1133
Vinyl Acetate Content 60 wt % Internal Method LP 015
General Purpose Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 20 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Vinyl Acetate Content 45 wt % Internal Method LP 015
General Purpose Grades
Property Nominal Value Test Method Condition Temperature
Melt Flow Index 190 °C 4 g/10mi ISO 1133
Vinyl Acetate Content 80 wt % Internal Method LP 015
General Purpose Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 27 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Vinyl Acetate Content 60 wt % Internal Method LP 015
General Purpose Grades
Property Nominal Value Test Method Condition Temperature
Mooney Viscosity 27 MU ISO 289 / ASTM D 1646 ML (1+4) 100 °C
Vinyl Acetate Content 70 wt % Internal Method LP 015